Low Melt fiber
Details
Specifications:2D,4D,6D,15D*38,51,64,76,89mm Characteristics: The fiber is produced by using polyester and modified polyester to spin simultaneously. The melting point is below 130℃. It can mix with normal fiber to form the nonwoven, then heat to bond them together and become an elastomer.
Use
Mattress of bed, seat cushions